10 m anode carbon block (19) Online Manufacturer
Thermal Conductivity: 120-150 W/mK
Porosity: 15-20%
Thermal Conductivity: 150-200 W/mK
Bulk Density: 1.55-1.75 G/cm3
Max. Working Temperature: 1800-2000℃
Flexural Strength: 10-14 MPa